TSLP | Sponge Iron | TATA Steel Long Product Limited
The crucial factor in this reduction process is the controlled combustion of coal and its conversion to carbon monoxide to remove oxygen from the iron ore. The overall production process inside the kiln requires a duration of 1012 hours during which the iron ore is reduced and discharged to a rotary cooler for cooling below 1000C, to prevent ...